Differential scanning calorimeter (DSC) studies showed that the m

Differential scanning calorimeter (DSC) studies showed that the melting point (T-m) and degree of crystallinity (X-c) of nylon 6/SiO2-COOH were lower than the pure nylon 6. Mechanical properties results of the nanocomposites showed that nylon 6 with incorporation of SiO2-COOH had better mechanical properties than that of pure nylon 6, nylon 6/SiO2, and nylon 6/SiO2-NH2. The morphology of SiO2, SiO2-NH2, and SiO2-COOH nanoparticles in

nylon 6 matrix was observed using SEM measurements. The results revealed that the dispersion of SiO2-COOH selleck screening library nanoparticles in nylon 6 matrix was better than SiO2 and SiO2-NH2 nanoparticles. (C) 2011 Wiley Periodicals, Inc. J Appl Polym Sci 122: 1316-1324, 2011″
“Electronic structures of perovskite oxides of SrMn1-xMoxO3 (0 <= x <= 0.75) have been investigated by employing soft x-ray absorption spectroscopy (XAS) and photoemission spectroscopy (PES). It is found that the valence states of Mn ions change systematically from Mn4+ for x = 0, to nearly Mn3+ for x = 0.3, and Mn2+ for x = 0.5, and then remain as Mn2+ for x >= 0.5. Both the Mo 3d core-level PES and Mo 3p XAS spectra show that the valence states of Mo ions remain unchanged as being hexavalent (Mo6+) for x <= 0.5 but that they decrease for x > 0.5 with increasing x. This study shows that Mo ions are mixed-valent for x > 0.5 in SrMn1-xMoxO3,

either with the Mo4+-Mo6+ configuration or with the Mo4+-Mo5+-Mo6+ configuration. (C) 2011 American Institute of Physics. [doi. 10.1063/1.3560890]“
“Background: Meat intake may be related selleck inhibitor to weight gain because of its high energy and fat content. Some observational studies have shown that meat consumption is positively associated with weight gain, but intervention studies have shown mixed results.

Objective: Our objective was to assess the association between consumption of total meat, red meat, poultry, and Akt inhibitor processed

meat and weight gain after 5 y of follow-up, on average, in the large European population who participated in the European Prospective Investigation into Cancer and Nutrition-Physical Activity, Nutrition, Alcohol, Cessation of Smoking, Eating Out of Home and Obesity (EPIC-PANACEA) project.

Design: A total of 103,455 men and 270,348 women aged 25-70 y were recruited between 1992 and 2000 in 10 European countries. Diet was assessed at baseline with the use of country-specific validated questionnaires. A dietary calibration study was conducted in a representative subsample of the cohort. Weight and height were measured at baseline and self-reported at follow-up in most centers. Associations between energy from meat (kcal/d) and annual weight change (g/y) were assessed with the use of linear mixed models, controlled for age, sex, total energy intake, physical activity, dietary patterns, and other potential confounders.

Comments are closed.